Styron A-Tech - PS-HI - Trinseo
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Styron A-Tech" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
... behaviour and good thermostability in the area of hot filling are required. While primarily the high-molecular GPPS grades are used in the transparent OPS sector, new high-toughness HIPS extrusion grades for packaging dairy products (example grade: Styron A-Tech 1200, manufacturer: Dow) have been developed with the goal of further improving the price performance ratio when mixed with suitable GPPS grades. Easier extrusion and better thermal mouldability of these mixtures should lead to producti...
Kunststoffe international, 2005-11-21, Rigid, Tough and Glossy all at Once
...ire polystyrene resins to have a performance profile that improves productivity, offers scope for lower wall thicknesses, permits a broader processing window and is less sensitive to external influences as a result of improved mechanical properties. Styron A-Tech polystyrene resins are impact-modified and also display a specially-adjusted rubber morphology. This permits improved stress distribution within the PS matrix. These new impact polystyrene resins are used in large appliances, for glossy...
Kunststoffe international, 2005-11-21, Teamwork Produces a New Design
...2000. The latest "Vitros" product line (title picture) is the result of intensive teamwork between Loewe, Videoplastic S.p.A (an injection-moulding company) and The Dow Chemical Company, which supplied the new high-impact polystyrene (grade: Styron A-Tech 1400). "Vitros" is Loewe's second line of television sets featuring a flat picture tube in combination with 100-Hz MediaPlus technology for totally flicker-free images and internet access. These TV designs presented new chal...
Kunststoffe international, 2007-10-21, Polystyrene (PS)
...side applications (caravans, window inserts, signs and the like). Dow is marketing an advanced high-impact grade polystyrene whose combination of toughness, gloss, stiffness and flow is adjusted via rubber morphology control (type: Styron A-Tech). Styrene-butadiene block copolymers (SBC) and their blends with polystyrene have been used for years in the production of highly transparent food packaging [2]. A new extrusion product (type: Styrolux HS 70) is being presented by BASF at the K show. It ...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.